The percentage of dissolved salts that a reverse osmosis or nanofiltration membrane removes from the feed water, calculated from feed and permeate concentrations.
Salt rejection is the standard measure of an RO membrane’s separating performance. It is calculated as SR (%) = (1 − Cp / Cf) × 100, where Cp is the permeate concentration and Cf is the feed concentration, usually measured as conductivity or total dissolved solids. Its complement is salt passage, SP (%) = 100 − SR, and operators trend salt passage because small changes are easier to read. A membrane that moves from 99.5 to 99.0 percent rejection has doubled its salt passage, from 0.5 to 1.0 percent. Rejection also varies by species: divalent ions such as calcium and sulfate are rejected more completely than monovalent sodium and chloride, and uncharged species such as boric acid pass more readily.
Salt passage depends on operating conditions as well as membrane condition. Water flux increases with net driving pressure, but salt flux is driven by the concentration difference across the membrane and is largely independent of pressure. Higher flux therefore dilutes the salt that passes and raises observed rejection, while higher recovery, higher temperature and concentration polarization lower it. Rejection data must be normalized before it can show a trend in membrane condition, and AWC’s cleaning guidance reads normalized salt passage together with normalized permeate flow and differential pressure. PROTON® models how salt passage shifts with flux at each stage of the array and calculates boron and arsenic rejection as functions of pH, temperature and ionic strength.
A sustained rise in normalized salt passage points to a change at the membrane surface. Oxidation of the polyamide layer by residual chlorine is a common cause, which is why chlorinated feed water is treated with dechlorination chemicals ahead of the RO unit. Delamination, O-ring and interconnector leaks, and damage from scale or fouling deposits produce the same symptom. Salt passage can also fall while permeate flow declines, since a light biological or organic film on the membrane can improve rejection. Where the cause is unclear, a membrane autopsy on the affected element identifies the damage mechanism directly.